Vacuum Plasma Spray Decomposition Of Titanium Particle/Glass-Ceramic Matrix Biocomposites

The vacuum plasma spray technique (VPS) has been successfully employed to coat Ti-6Al-4V substrates with bioactive glasses and Ti particle/glass-ceramic matrix biocomposites. The composites were prepared by sintering, under an Ar flow, green bars of bioactive glass powders and 30% volume Ti particles. Each coating was found to be bioactive and well bonded to the substrate; the composites showed better mechanical properties than the pure glass matrices and the hydroxylapatite coatings deposited by the same VPS technique.

Author
M Ferrarris Et Al
Origin
Polytechnic Of Torino, Italy
Journal Title
J Am Ceram Soc 79 6 1996 1515-1520
Sector
Glass Ceramics
Class
GC 244

Request article (free for British Glass members)

Vacuum Plasma Spray Decomposition Of Titanium Particle/Glass-Ceramic Matrix Biocomposites
J Am Ceram Soc 79 6 1996 1515-1520
GC 244
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.