Uv Protection For Container Glassware

A coating system that affords protection against high energy radiation in the near ultraviolet part of the spectrum is described.

Author
P Bottger
Origin
Deco-Glass P Bottger Kg
Journal Title
Glass International March 1989 41
Sector
Container glass
Class
C 193