Uv Ink System Developed For Glass Finishing

A new, environmentally-friendly UV ink system has been developed for the decoration of drinking glasses and bottles. Marabu's new UV ink system is a heavy metal-free, offers energy savings because of UV curing, and has a wide range of brilliant colour shades. Its main advantages are: brilliant high-gloss colours; high printing speeds and shorter curing times; good adhesion and scratch resistance; outstanding resistance to chemicals. For more information please see: www.marabu-inks.com or email: [email protected]

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide March-April 2006 36-37
Sector
Container glass
Class
C 2920

Request article (free for British Glass members)

Uv Ink System Developed For Glass Finishing
Glass Worldwide March-April 2006 36-37
C 2920
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.