Utilization Of Fly Ash For The Production Of Crockery And Novelty Wares

The feasibility of using fly ash, a waste inorganic product obtained by the combustion of coal in boilers of thermal power plant, was studied for the development of value added glazed ceramic materials such as crockery and novelty wares. Progressive incorporation of fly ash in replacement of silica and potash feldspar in the standard crockery ware body compositions resulted in an increase in unfired and fired strengths coupled with vitrification at 1250 deg C up the the addition of 30% fly ash. Further incorporation of fly ash, up to 50% showed a decrease in fired strength and increase in water absorption at the same temperature. Improved stoneware crockery body utilising 30% fly ash in the standard body composition was successfully produced.

Author
S K Mukherji Et Al
Origin
Cgcri, India
Journal Title
Trans Indian Ceramic Soc 60 4 2001 182-186
Sector
Glass Ceramics
Class
GC 482

Request article (free for British Glass members)

Utilization Of Fly Ash For The Production Of Crockery And Novelty Wares
Trans Indian Ceramic Soc 60 4 2001 182-186
GC 482
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 18 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.