Utilisation Of Cement Waste Products To Produce Glasses And Glass-Ceramics

During recent years special attention has been devoted to solving pollution problems during the manufacture of cement. Large amounts of waste substances are produced during manufacture and recycling represents the best option to reduce or minimise pollution. Laboratory studies have been performed using cement wastes, together with other common raw materials to produce glass with the appropriate compositions.

Author
H A Elbatel And N A Ghoneim
Origin
National Research Center, Cairo, Egypt
Journal Title
5Th Int Otto Schott Colloquium, Jena, July 1994 380-383
Sector
General
Class
G 1267

Request article (free for British Glass members)

Utilisation Of Cement Waste Products To Produce Glasses And Glass-Ceramics
5Th Int Otto Schott Colloquium, Jena, July 1994 380-383
G 1267
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.