Using Lasers For Glass Decoration And Marking

Glass marking continues to fuel the expansion of the CO2 laser market. Although most glass marking is centred around automotive, commercial, industrial and residential window glass, there are also many applications for marking glass bottles and other decorative consumer items, as explained in this article.

Author
Un-named
Origin
Unknown
Journal Title
Glass International November 2012 32-33
Sector
General
Class
G 4066

Request article (free for British Glass members)

Using Lasers For Glass Decoration And Marking
Glass International November 2012 32-33
G 4066