Using Langmuir-Blodgett Techniques To Deposit Cobalt Phthalocyanine Films Onto Glass Or Quartz Slides And Subsequent Axial Coordination Of Basic Ligands

Introduction of ligands or spacers on phthalocyanine (Pc) structure was planned and confirmed by different physical techniques. Mononuclear structures, dimers & oligomers of 2,9,16,23-tetra(neopentoxy)phthalocyanine of cobalt (CoTnPc) (D4h) (high spin) and CoTnPc/L (C4v) (low spin) (L=axial ligand; i.e. cyanide, pyridine, 4-cyano-pyridine, pyrazine and 4,4'-bipyridyl) were preapred as solid compounds or as film structures and characterised by using elemental analysis, 1H NMR, IR and electronic spectra.

Author
N A Wiederkehr
Origin
Fisico Quimica, Brazil
Journal Title
Phys Chem Glasses 49 6 2008 326-333
Sector
Special Glass
Class
S 3537

Request article (free for British Glass members)

Using Langmuir-Blodgett Techniques To Deposit Cobalt Phthalocyanine Films Onto Glass Or Quartz Slides And Subsequent Axial Coordination Of Basic Ligands
Phys Chem Glasses 49 6 2008 326-333
S 3537
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.