Using Industrial Waste In Boron-Free And Fluorine-Free Ground Enamels

The feasibility of using bottle cullet and carbonate ores in the production of enamels for use on steel components of domestic appliances has been demonstrated.

Author
A V Sarukhanishvili, I G Zedginidze
Origin
Georgian V I Lenin Polytechnical Institute
Journal Title
Glass And Ceramics 1987 44 3-4 137-139