Use Of Thermally Inertized Cement-Asbestos For The Production Of Rock/Glass Wool (In Italian)

In this study, the recycling of the product of thermal decomposition of cement-asbestos for the production of rock/glass wool is presented. The material, treated at 1200 deg C displays a full re-crystallisation of the asbestos fibres into innocuous Mg-, ca-rich silicates to be recycled. To formulate the blend for the glass/rock wool production, the thermally treated cement-asbestos was diluted with a low-cost feldspar from Sardina and a low-cost red clay from the Northern Apennines. The mineralogical, physical-chemical and technological properties of the synthesised glasses was tested and it was demonstrated that they are totally comparable with production standards.

Author
G Torri & A F Gualtieri
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 37 4 2007 17-24
Sector
Glass Fibre
Class
GF 550

Request article (free for British Glass members)

Use Of Thermally Inertized Cement-Asbestos For The Production Of Rock/Glass Wool (In Italian)
Riv Staz Sper Vetro 37 4 2007 17-24
GF 550
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.