Use Of Reactive Gases In The Tempering Process Towards Ultra-Thin Glasses For Solar Energy Applications

The LIMES project (Light Innovative Materials for Enhanced Solar Efficiency) is a fruitful collaboration to optimise many different properties in state-of-the-art solar glasses for photovoltaic (PV) modules. The bulk optical properties are optimised by adding fluorescent elements that absorbs harmful UV-radiation whole increasing the overall efficiency in the visible part of the solar spectrum. Functional coatings that are both anti-reflective and self-cleaning are being studied. This work investigates routes to achieve thin thermally toughened cover glasses with enhanced mechanical and chemical properties. A promising route to achieve this is by thermal toughening in reactive gases.

Author
P Sundberg Et Al ([email protected])
Origin
Glafo, Sweden
Journal Title
13Th Symp Eu Soc Of Glass Science 2016 289-291
Sector
Special Glass
Class
S 4337

Request article (free for British Glass members)

Use Of Reactive Gases In The Tempering Process Towards Ultra-Thin Glasses For Solar Energy Applications
13Th Symp Eu Soc Of Glass Science 2016 289-291
S 4337
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.