Use Of Optical Oxygen Sensors To Monitor Residual Oxygen In Pre- & Post-Pasteurised Bottled Beer & Its Effect On Sensory Attributes & Product Acceptability During Simulated Commercial Storage

Disposable optical oxygen sensors were used to non-destructively assess the levels of residual oxygen in the headspace of commercially produced Lager beer in 330 ml clear glass bottles. Monitored before and after pasteurisation, oxygen concentration was observed to drop as oxygen diffused into the beer. Oxygen levels between 0% and 5% were present in the bottle headspace pre-pasteurisation. Oxygen diffusion into the beer was monitored over time under refrigeration (~4 °C) and a sensory panel was used to determine the effect of residual oxygen on the sensory quality of the beer. The headspace in the bottles was also monitored over time where oxygen increased to a level of ~0.5% on average over the course of the shelf life. Interestingly, results showed that beer samples possessing higher levels of oxygen present prior to pasteurisation also possessed the most negative sensory attributes associated with the beer, particularly those consistent with beer staling. The developed optical sensor was shown to act as a predictor of sensory quality and may have on-line applications in the beer packaging sector.

Author
Un-named
Origin
Unknown
Journal Title
Lwt - Food Science & Technology 50 1 Jan 2013 226-231
Sector
Container glass
Class
C 4919

Request article (free for British Glass members)

Use Of Optical Oxygen Sensors To Monitor Residual Oxygen In Pre- & Post-Pasteurised Bottled Beer & Its Effect On Sensory Attributes & Product Acceptability During Simulated Commercial Storage
Lwt - Food Science & Technology 50 1 Jan 2013 226-231
C 4919
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.