The Use Of Microwave Energy For The Firing Of Heavy Clay Products

Thermal analyses and dielectric property measurements of numerous heavy clay bodies provided data for the selection of optimum body compositions. The addition of carbon increased the complex permittivity of the bodies tested, in such a way that it improved the efficiency of microwave coupling in the firing process. The Microwave Autogenous Firing (MWAF) mechanism was identified. The key variables that influenced this microwave heating process were examined.

Author
G Tayler Et Al
Origin
Acme Brick Co, Usa
Journal Title
Proc Int Microwave Power Inst Heating Symposium April 2001 27-32
Sector
Special Glass
Class
S 2440

Request article (free for British Glass members)

The Use Of Microwave Energy For The Firing Of Heavy Clay Products
Proc Int Microwave Power Inst Heating Symposium April 2001 27-32
S 2440
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.