The Use Of A Khl-69 Chromatography For The Analysis Of Gases In Bubbles In Glass

A gas chromatographic technique for analysing gases in optical glass seed is described. Separation of H2, O2, N2 and CO is effected on a molecular sieve and CO2 and C2H2 on silica gel. The results of the analyses are reported.

Author
Aa Koryavin Et Al
Origin
Unknown
Journal Title
Glass And Ceramics 33 1-2 1976 25-27