The Use Of Ion Selective Electrodes For Analysis Of Sodium And Calcium In Glass Batch

Commercially available sodium and calcium ion selective electrodes can be used to determine quantitative occurrences of acid soluble sodium and calcium source materials in glass batch. Performance characteristics of each specific ion electrode are described and guidelines are set forth for development of the analytical technique.