Use Of Cobalt-Containing Oxide Waste For Synthesizing Enamels

It is shown that introduction of up to 7 wt% cobalt-containing oxide catalyst waste into the mixtue for synthesizing acid-resistant one-coat enamel does not worsen its wettability. The content of cobalt in such an enamel amounts to 0.2-0.3 wt%, which is sufficient for its satisfactory cohesion with steel.