The Use Of Ceramic Welding To Extend The Life Of A Furnace

The method used for ceramic welding is described and a detailed account follows of the maintenance schedule of a particular furnace.

Author
T S Busby, J R Mackintosh
Origin
Foseco (Fs) Ltd
Journal Title
Glass Technology 33 4 August 1992 112-116
Sector
Refractories
Class
R 89

Request article (free for British Glass members)

The Use Of Ceramic Welding To Extend The Life Of A Furnace
Glass Technology 33 4 August 1992 112-116