The Use Of Calcium Hydroxide With Special Characteristics In Glass Furnace Flue Gas Treatment With Recovery Of Dust Into Glass Batch

After analyzing the factors that affect the chemico-physical characteristics of lime, a few examples of its use in semi-dry and dry flue gas abatement systems are presented, both in laboratory and in pilot and industrial plants. The efficiency of abatement varies with two physical parameters - humidity and temperature of flue gas - and with one engineering parameter - the amount of residual free lime recycled. Examples are also presented on the impact of hydrated lime specific surface on desulfurization efficiency; industrial applications in the glass industry and related issues are also illustrated.

Author
L Cariboni & F Mereu
Origin
Icico Srl, Italy
Journal Title
Int Glass Journal No 109 2000 59-64
Sector
General
Class
G 2280

Request article (free for British Glass members)

The Use Of Calcium Hydroxide With Special Characteristics In Glass Furnace Flue Gas Treatment With Recovery Of Dust Into Glass Batch
Int Glass Journal No 109 2000 59-64
G 2280
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.