Use Of Amorphous Alumino-Silicate Wool/Refractory Ceramic Fibres (Asw/ Rcf) In The European Glass Industries

The European glass industries (comprising flat glass, container glass, domestic glass, continuous filament glass fibres and special glass) need alumino-silicate refractory ceramic fibre (ASW/RCF) products with very limited possibilities to use alternative materials. ASW/RCF, in the form of mats, are used in the glass melting process as insulation material for moulds (covering & interior wall insulation), mould release agents, transport media, and tool protection. Alternative materials have been investigated, but to date no suitable material has been found that can withstand the high thermal, chemical and mechanical stress experienced in the high temperature glass melting process. ASW/RCF blankets and other products in high-temperature melting glass processes are electrical and thermal insulation of platinum components, sealing of floor drains in the glass melting tank, sealing of electrode feeders and permanent insulation of the expansion joints between the melting tank and the plate block. This material is also used for temporary repairs like covering small holes in the roof or crown of a melting tank, and gaps in the rear and side wall. Other mats are used to insulate the glass feeder, the stirring unit and various parts during hot repairs. Therefore, the production of many glass types is not currently possible without products based on ASW/RCF as insulation material. Employees in the glass industry are experienced and trained in dealing with ASW/RCF. The working areas are monitored regularly by the Member States’ competent authorities, such as the Employer's Insurance Association (Verwaltungs-Berufsgenossenschaft VBG) in Germany. No occupational diseases have been recorded after more than 50 years of use. The use of ASW/RCF products is restricted to an absolute minimum since substitution is mandatory after classification in 1997.

Author
Glass For Europe
Origin
Unknown
Journal Title
www.Glassallianceeurope.Eu/Images/Cont/Gae-Paper-On-Rcf-March-2013_File.Pdf
Sector
General
Class
G 4143

Request article (free for British Glass members)

Use Of Amorphous Alumino-Silicate Wool/Refractory Ceramic Fibres (Asw/ Rcf) In The European Glass Industries
www.Glassallianceeurope.Eu/Images/Cont/Gae-Paper-On-Rcf-March-2013_File.Pdf
G 4143
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.