Us Takes The Lead - Diamond And Dlc Films R&D And Markets

After a gestation period of one decade, followed by another decade of commercial development and growth in niche markets, the US has taken the lead in technology for producing diamond coatings and thin films at low temperatures and pressures - and at relatively low cost.