Upgraded Crown Insulation Leads To Fuel Savings

Lubisol Engineering has 20 years experience in the field of thermal insulation and hermetic sealing of glass furnace silica crowns. As a result of its studies, the company concluded that the standard crown insulation can and should be further improved.