Upconversion Luminescence Of Er3+ Doped Fluoride Glasses

In this paper the spectroscopic and fluorescence properties in Er3+ ions in ZBLAN fluoride glass were studied as a function of chlorine content and dopant concentration. The results show the anions have much more effect on the fluorescence properties. The upconversion fluorescence in visible region was measured using 800nm Ti: sapphire laser as excitation source. A strong green upconversion fluorescence band at 550nm for transition is observed in all samples.

Author
H Hefang Et Al
Origin
Shanghai Inst Of Optics And Fine Mechanics, China
Journal Title
Proc Of Xvi Icg, Beijing, China Vol7 1995 234-239
Sector
Special Glass
Class
S 1501

Request article (free for British Glass members)

Upconversion Luminescence Of Er3+ Doped Fluoride Glasses
Proc Of Xvi Icg, Beijing, China Vol7 1995 234-239
S 1501
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.