Upconversion Fluorescent Glasses

The effect of doping concentration, host glass composition, co-doping ion and temperature on the upconversion fluoresence of Er3+ doped fluoride glasses in order to understand the upconversion excitation mechanism for both 800nm and 980nm diode laser pumping is described.

Author
H Toratini Et Al
Origin
Hoya Corp, Japan
Journal Title
Rivista Della Staz Sper Vetro 23 1 1992 31-34
Sector
Special Glass
Class
S 672

Request article (free for British Glass members)

Upconversion Fluorescent Glasses
Rivista Della Staz Sper Vetro 23 1 1992 31-34
S 672