Unusual Plasticization For Structural Relaxed Bulk Metallic Glass

Unusual plasticization for structural relaxed CuZr-based bulk metallic glass (BMG) has been found. Even though thermal-annealing usually leads to unfavourable relaxation-induced embrittlement for most BMGs, this BMG exhibits an improved plasticity after annealing. This behaviour is attributed to an evolution of nanolevel hetereogeneity for this unstable or heterogeneous BMG. Less initiation of shear bands by structural relaxation and evolution of heterogeneity from thermal-annealing are considered to contribute cooperatively to the plasticity of relaxed glass. This study provides a new viewpoint to improve the mechanical properties of BMGs upon relaxation, in which a microstructural heterogeneity is distributed among a glassy matrix. This finding may also expand the applications of BMGs as promising structural materials because of unusual resistances to annealing-embrittlement.

Author
W Guo Et Al
Origin
Tohoku Unviersity, Sendai, Japan
Journal Title
Materials Science & Engineering A 699 2017 81-87
Sector
Special Glass
Class
S 4378

Request article (free for British Glass members)

Unusual Plasticization For Structural Relaxed Bulk Metallic Glass
Materials Science & Engineering A 699 2017 81-87
S 4378
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
6 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.