A Unified Materials Approach To Mitigating Optical Nonlinearities In Optical Fibre. I. Thermodynamics Of Optical Scattering

Sustained progress in the development of optical fibres has led to the present state where further improvements in performance are limited by intrinsic optical nonlinearities. In order to circumvent such limitation,s the user community has adopted two general approaches: (i) engineer the enabled systems accordingly; and/or (ii) microstructure the fibre to shift nonlinear thresholds to high optical power levels. In both cases, the nonlinearities are accepted as they are and performance is enhanced through added system or fibre design complexity. This is the first paper in a series of three.

Author
J Ballato Et Al
Origin
Clemson University, Sc, Usa
Journal Title
Applied Glass Science May 2018 263-277
Sector
Glass Fibre
Class
GF 750

Request article (free for British Glass members)

A Unified Materials Approach To Mitigating Optical Nonlinearities In Optical Fibre. I. Thermodynamics Of Optical Scattering
Applied Glass Science May 2018 263-277
GF 750
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.