Ultrathin Glass Record Smashed As Slim Becomes Vogue

China has set a new world record for thinness with its ultra-thin glass, with an expert saying that the core technology breakthrough in manufacturing makes China at par when dealing with foreign companies, and also makes the international market a fair one. According to China Central TV, the new glass is 0.12mm thick and is produced by the float process.Developed by Bengbu Glass Industry Design Research Institute in East China's Anhui Province, the glass began mass production April 2018, the report said.

Author
Un-named
Origin
Unknown
Journal Title
Asian Glass No 3/2018 6
Sector
News Items
Class
N 3916a