Ultrasonic Roll Seam Welding For The Production Of Glass/Metal Compounds

Joining technology of glasses and glass-ceramics with metal is growing in importance in view of increased application possibilities of such compounds in the machinery and electronics industries. A new method has recently come into competition with the current production method. This novel method is ultrasonic welding. So far this technology has only been applied in ultrasonic spot welding. However, it is now possible to manufacture compounds with a shear strength of up to 50 MPa at low temperatures (

Author
D Eifler Et Al
Origin
Lehrstuhl Fur Werkstoffekunde, Germany
Journal Title
Glastech Ber Glass Sci Technol 69 10 1996 326-330
Sector
General
Class
G 1531

Request article (free for British Glass members)

Ultrasonic Roll Seam Welding For The Production Of Glass/Metal Compounds
Glastech Ber Glass Sci Technol 69 10 1996 326-330
G 1531
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.