Ultrasonic Measurements And Complex Elastic Moduli Of Silicate Glass Melts In The Viscoelastic And Viscous Range

The temperature and frequency-dependence of the ultrasonic velocity and attenuation in glass melts is investigated up to a temperature of 1400 deg. C by means of an equipment for measuring the longitudinal and transversal ultrasonic waves.

Author
H Bornhoft & R Bruckner
Origin
Technische Universitat Berlin, Germany
Journal Title
Glastech Ber Glass Sci Technol 67 9 1994 241-254