Ultrafast Optical Switches And Wavelength Division Multiplexing (Wdm) Amplifiers Based On Bismuth Oxide Glasses

Glasses with a high refractive index exhibit interesting properties. All optical switching and broadband amplification performances have been demonstrated using glasses based on bismuth oxide (Bi203). Optical Kerr shutter (OKS) switching and degenerated four-wave mixing experiments for nonresonant-type Bi203-B203-Si02 glasses have been performed using femtosecond lasers. This glass exhibits an ultra-fast response in OKS operation. Moreover, terahertz-range optical switching has been successfully performed with this glass, using a 1.5-THz pulse train.

Author
N Sugimoto
Origin
Asahi Glass, Japan
Journal Title
J Am Ceram Soc 95 5 2002 1083-1088
Sector
Special Glass
Class
S 2369

Request article (free for British Glass members)

Ultrafast Optical Switches And Wavelength Division Multiplexing (Wdm) Amplifiers Based On Bismuth Oxide Glasses
J Am Ceram Soc 95 5 2002 1083-1088
S 2369
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.