Ultra High Temperature Ceramic Coatings For Oxidation Protection Of Carbon-Carbon Composites (Abstract Only - Article Available To Members Online Via: www.Ceramic.org)

Carbon-carbon composites are attractive materials for hypersonic flight vehicles, but they oxidize in air at high temperatures. Corral and Loehman investigated the use of multilayers of high-temperature ceramics, such as ZrB2 and SiC as continuous and adherent thermal protection coatings.

Author
E L Corral & R E Loehman
Origin
Unknown
Journal Title
Am Ceram Soc Bull
Sector
Glass Ceramics
Class
GC 699

Request article (free for British Glass members)

Ultra High Temperature Ceramic Coatings For Oxidation Protection Of Carbon-Carbon Composites (Abstract Only - Article Available To Members Online Via: www.Ceramic.org)
Am Ceram Soc Bull
GC 699
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.