Tv Oxy-Fuel Conversion And Experience With Noncatalytic Denitrification

Schott Glas in Mainz operates three TV tanks. Until 1996, all three were regenerative cross-fired tanks. The two TV panel tanks used to run with mixed gas/oil underport firing, and the TV funnel tank ran with gas sideport firing. The TV panel tanks had already been rebuilt with a catalyzer system for NOx abatement when the discussion about oxy-fuel conversion just started. The decision was made to go with the catalysator for costs and quality issues. The one tank without a de-NOx device until 1996 was the TV funnel tank.

Author
M R Lindig
Origin
Schott Glas, Germany
Journal Title
Ceram Eng Sci Proc 20 1 1999 37-45
Sector
General
Class
G 3634

Request article (free for British Glass members)

Tv Oxy-Fuel Conversion And Experience With Noncatalytic Denitrification
Ceram Eng Sci Proc 20 1 1999 37-45
G 3634
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.