[Turkey] Pasabahce Lehr Investments

Car-Met has received further equipment orders from Pasabahce Cam Sanayii for the glassmaker's latest investments in Turkey, Bulgaria and Russia. This agreement is the result of a long relationship between the Italian hollow glass lehr manufacturer and the Turkish glassmaker. The investment consists in 20 lines for tableware production. Five are for Turkish plants in Kirklarelia, Eskisehir and Mersin, six to the Trakya plant in Bulgaria, and nine for Nizhny Novgorod plant in the Russian Federation. Each project involves several annealing lehrs of different sizes and a special decorating lehr with a direct and indirect heating system, developed specially to assure top quality in tableware decoration and working with heavy metals colours.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Sept-Oct/2013 14
Sector
Domestic glass
Class
D 1314

Request article (free for British Glass members)

[Turkey] Pasabahce Lehr Investments
Glass Worldwide Sept-Oct/2013 14
D 1314
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.