Trends In Refractory Technology

Developments in the refractories market and technology are reviewed. These include new dense chromic oxide and zircon refractories from Corhart and high-zirconia fusion cast materials from SEPR. Environmental issues concerning the disposal of chrome-containing refractories are also discussed.

Author
G Geiger
Origin
Unknown
Journal Title
Ceramic Bulletin 1991 70 6 994-1003
Sector
Refractories
Class
R 68