Trends In Homogeneous Crystal Nucleation In Oxide Glasses

Calculations have been performed to estimate the temperature of maximum nucleation rate for several oxide glasses.

Author
E D Zannotto, M C Weinberg
Origin
University Of Arizona
Journal Title
Phys Chem Glasses 1989 30 5 186-192
Sector
Special Glass
Class
S 314

Request article (free for British Glass members)

Trends In Homogeneous Crystal Nucleation In Oxide Glasses
Phys Chem Glasses 1989 30 5 186-192
S 314