Treatment Of Sulphate Leach Liquors To Recover Cobalt From Waste Dusts Generated By The Glass Industry

A hydrometallurgical process has been developed for cobalt recovery from a waste dust formed during the colouring of glass plates. This dust, containing about 33% Co, is highly contaminated by Fe and Cr. The process consists of the following steps: Leaching the dust in H2SO4; Purification of leach liquors by hydrolytic precipitation using Na2CO3 and/or K2CO3 as neutralising agent; Precipitation of basic cobalt(II) carbonate; Dissolution of basic cobalt(II) carbonate in sulphuric acid and separation of residual chromium; Electrowinning of cobalt from refined sulphate solutions. A compact metallic deposit containing >99.5% Co was obtained.

Author
J Jandova Et Al
Origin
Institute Chemical Technology, Prague
Journal Title
Hydrometallurgy 77 2005 67-73
Sector
Special Glass
Class
S 2963

Request article (free for British Glass members)

Treatment Of Sulphate Leach Liquors To Recover Cobalt From Waste Dusts Generated By The Glass Industry
Hydrometallurgy 77 2005 67-73
S 2963
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.