Treatment Of Glass Furnace Waste Gases - Combined Separation Of Dust And Gaseous Pollutants

Italian legislation and the EU norms require improvments in both dust collection and emissions from glass furnaces. Proper design of dust collection systems presupposes a clear knowledge of the characteristics of the dust. Most glass producers have chosen to build plants with dry process treatment, equipped with electrostatic precipitators because of reliability, low maintenance and wide work flexibility.

Author
G Bonetti
Origin
Lurgi Spa, Italy
Journal Title
International Glass Journal No 88 1996 28-34
Sector
General
Class
G 1460

Request article (free for British Glass members)

Treatment Of Glass Furnace Waste Gases - Combined Separation Of Dust And Gaseous Pollutants
International Glass Journal No 88 1996 28-34
G 1460
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.