Transport Characteristics Of Ceramic Particles During Compaction

Transport characteristics during the compaction containing powders of ceramic particles, expressed as mass conductives derived from quasi-diffusion coefficients have been analysed.

Author
M Radeka Et Al
Origin
Unknown
Journal Title
Cfi/Ber Dkg 77 4 2000 24-29
Sector
Glass Ceramics
Class
GC 376

Request article (free for British Glass members)

Transport Characteristics Of Ceramic Particles During Compaction
Cfi/Ber Dkg 77 4 2000 24-29
GC 376