The Transport And Settling Of Platinum-Group-Metal Particles In Glass Melts

This work is linked with the development of models and numerical simulations of High-Level-Waste (HLW) vitrification processes. Platinum-Group-Metals (PGM) are found in the vitrification process of nuclear waste as fission products. During the melting, the glass generally shows a homogenous liquid phase seeded with non-soluble heavy platinum-group-metals particles mainly made of palladium and ruthenium dioxide. Previous studies reported large spatial discrepancies of the local volume fraction of particles int he melt because of particles settling with time. This migration of particles towards poorly agitated bottom parts of the crucible impacts the dynamical, electrical and thermal state of the melt because of concentration-dependent electrical conductivity and viscosity of the suspension. A theoretical one-fluid transport model is derived with little hypothesis, with particular attention paid to the hindered settling term. The resulting unsteady transport equation has shown to account for observed volume fraction profiles in seeded glass heat treated at different temperatures and for different time horizons. These experiments have been carried out wit a HLW glass simulate and we measured PGM particles local concentration using Laser Induced Breakdown Spectroscopy. We investigate both isothermal and non-isothermal settling and special attention is given to the temperature dependence of Stokes terminal settling velocity and particles diffusivity due to temperature dependent glass viscosity. The model can easily be coupled with existing 3D thermo-hydraulic numerical codes, thus enhancing the precision of heat flux predictions between the melt and the crucible. The full model will eventually help designing crucibles with reduced PGM retention.

Author
G B Rossa & E Sauvage
Origin
Cea, Den, Dtcd, Scdv, Ldpv, France
Journal Title
13Th Sympof Eu Soc Of Glass Science 2016 14-15
Sector
Special Glass
Class
S 4317

Request article (free for British Glass members)

The Transport And Settling Of Platinum-Group-Metal Particles In Glass Melts
13Th Sympof Eu Soc Of Glass Science 2016 14-15
S 4317
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.