Transparent Yag Ceramics

Konoshima Chemical Co Ltd, has been developing transparent ceramics since the 1980s, yttrium-aluminium-garnet (YAG) ceramic being one of them. Since the beginning of the development process, Konoshima researchers have collaborated with researchers at the National Institute for Materials science, Japan. In order to obtain high transparency, the company fabricates YAG ceramic using in-house-developed high-purity raw materials. Specifically, the YAG precursor is fabricated by wet chemical synthesis and calcined to obtain YAG powder. After milling, a desired form is obtained by the slip casting method. Finally, highly transparent YAG ceramic is obtained by the traditional sintering process.

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 84 5 2005 9
Sector
Glass Ceramics
Class
GC 624

Request article (free for British Glass members)

Transparent Yag Ceramics
Am Ceram Soc Bull 84 5 2005 9
GC 624
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 19 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.