Transparent Glass-Ceramics Obtained During Cooling

This paper examines the microstructure of glass-ceramics obtained during cooling melts of different compositions in the ternary Li20-Al203-Si02 system.

Author
C Siligardi Et Al
Origin
University Of Modena, Italy
Journal Title
Glastech Ber Glass Sci Technol 73 C1 2000 213-220
Sector
Glass Ceramics
Class
GC 514