Transparent B-Willemite Glass-Ceramics

Transparent glass-ceramics based on crystals of b-willemite solid solution can be obtained in the SiO2-Al2O3-ZnO-K2O-Na2O system. The glass-ceramics are self-nucleating via liquid-liquid phase separation and therefore require no added nucleating agents. Because they offer only tetrahedral and small intersitial sites, b-willemite crystals can serve as hosts for small, optically-active transition elements such as Cr4+. Fluorescence measurements of Cr-droped glass-ceramics based on b-willemite indicated strong Cr4+ emission over a broad range of wavelengths (1100-1700 nm).

Author
L R Pinckney
Origin
Corning Inc, Usa
Journal Title
Glastech Ber Glass Sci & Technol 73 C1 2000 329-332
Sector
Glass Ceramics
Class
GC 807

Request article (free for British Glass members)

Transparent B-Willemite Glass-Ceramics
Glastech Ber Glass Sci & Technol 73 C1 2000 329-332
GC 807
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.