Transmutation Of Actinides

An advanced process has been developed on a laboratory scale at the Institute for Transuranium Elements for the fabrication of transmutation fuels and targets. The process consists of the fabrication of highly porous beads using a sol-gel method, their infiltration by a nitrate solution of the relevant actinide, and calcination, compaction, and sintering to give the final product pellets. This work presents the results obtained in the qualification of this process whereby dense paritally-yttria-stabilized zirconia pellets with high contents of cerium and plutonium have been fabricated.

Author
A Fernandez Et Al
Origin
Inst Transuranium Elements, Germany
Journal Title
Jacs 85 3 2002 694-696
Sector
Special Glass
Class
S 2568

Request article (free for British Glass members)

Transmutation Of Actinides
Jacs 85 3 2002 694-696
S 2568
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.