Transmited And Reflected Distortion Of Float And Laminated Glass

Optical distortion is an important quality parameter in float glass production and fabrication. Transmitted and reflected distortion individually as well as their relationship in combination need to be understood and monitored to guarantee an acceptable product quality. This paper explains the physical phenomenon, the adaptation of measurement techniques and parameters which can be important in determining final product quality.

Author
U Pingel & P Ackroyd
Origin
Isra Glass Vision, Germany
Journal Title
65Th Conference On Glass Problems 2004 25-35
Sector
Flat glass
Class
F 1830

Request article (free for British Glass members)

Transmited And Reflected Distortion Of Float And Laminated Glass
65Th Conference On Glass Problems 2004 25-35
F 1830
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.