Transformation Toughening Of Machineable Mica Glass Ceramics

A new two-step heating process was recently developed for the strengthening of mica glass ceramics. Two mechanisms of subsequent toughening were applied by the second heat treatment: (i) the crystallization of a second silicate phase (i.e. anorthite) and (ii) the transformation toughening by addition of Zr02. Transmission-electron-microscopy (TEM) studies were performed to investigate in detail the microstructure development in this two-step heating process. In principle, the crystallization mechanisms were found to be similar for all samples investigated. However, the resulting microstructures differed significantly even after small compositional changes.

Author
M Reise Et Al
Origin
Fraunhofer-Inst Silicatforschung, Germany
Journal Title
Proc Xvii Icg Vol 5 Beijing 1995 241-246
Sector
Glass Ceramics
Class
GC 421

Request article (free for British Glass members)

Transformation Toughening Of Machineable Mica Glass Ceramics
Proc Xvii Icg Vol 5 Beijing 1995 241-246
GC 421
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.