The Transfer Of Glass - Part 1: Transfer Of Glass To Individuals At Different Distances

Studies have been carried out to investigate the number of glass fragments transferred to the clothing of a person in the vicinity of a breaking window. Clothed tailor's dummies were subjected to flying debris from window breaking.