Tin Penetration Profile In The Bottom Surface Of Alkali-Free Aluminoborosilicate Float Glass

Tin penetration profile in the bottom surface of alkali-free aluminoborosilicate glass (AFAB), which was manufactured by the float process, was recorded on a secondary ion mass spectrometry (SIMS) in comparison with that of soda-lime-silicate glass (SLS). According to the results, there was no apparent "hump" in AFAB while it was observed in SLS.

Author
T Mukai Et Al
Origin
Asahi Glass, Japan
Journal Title
Icg 2 Extended Abstracts 2001 38-39
Sector
Special Glass
Class
S 2261