Tin Influence On The Thermo-Mechanical Behaviour Of Silica-Soda-Lime Glass

In this paper the author has elaborated the silica-soda-lime glass with uniform concentrations of tin. Some physical properties have been measured. The extrapolation to the thermo-mechanical behaviour of the tin side of float glass is then proposed and discussed.