Tin Bath Periscope System

The Lenox tin bath periscope system provides real-time, high-resolution images in the tin bath environment. A specially designed & proven water-jacketed lens assembly enables operation in this hostile environment. Used by glass manufacturers, it monitors and records the amount of trim being produced, the wheel depth and tracking, the function of the automated drive system and the top knurl wheels. The complete remote viewing package includes the lens systems and water jacket, camera housing, and CCD black and white camera. The lens system has a 2.5" OD, and is available in 8-ft & 10ft lengths. The system provides a 30 degree field of view at a right-angle direction. For more information please email: [email protected]

Author
Un-named
Origin
Unknown
Journal Title
Am Ceram Soc Bull 85 8 2006 42
Sector
News Items
Class
N 1991

Request article (free for British Glass members)

Tin Bath Periscope System
Am Ceram Soc Bull 85 8 2006 42
N 1991
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 12 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.