The Time-Dependent Change Of Radiation-Induced Optical Band As Criteria Of Glass Disordering

The evolution of the spectral shape of the radiation-induced optical band of the deep level defect in amorphous and glassy material was simulated using a computer taking into account microscopic structure of the defect. The model suggest that the energy of local phonon connected with the defect has a wide distribution through glass martrix at short times after the irradiation pulse due to the presence of random local strains in the disordered atomic network of the glass.

Author
A Diikov
Origin
S I Vavilov State Optical Inst, Russia
Journal Title
Ceramic Trans 82 1998 335-340
Sector
Special Glass
Class
S 1623a

Request article (free for British Glass members)

The Time-Dependent Change Of Radiation-Induced Optical Band As Criteria Of Glass Disordering
Ceramic Trans 82 1998 335-340
S 1623a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.