Tiama Partnership

Stoelzle Czestochowa, part of Austria's Stoelzle Glass Group, has formed a partnership with Tiama MSC & SGCC for the installation of four inspection machines dedicated to the inspection of premium spirit containers. The new equipment was approved by Stoelzle after several months of online benchmarks, allowing the Polish Glassworks to test new quality inspection systems from various manufacturers in the field of sidewall, base, finish and mould number reader. The concept that combines MULTI5, Kompass & MCAL4 allows a perfect control of special shapes, while orienting the containers with the help of software tools.

Author
Un-named
Origin
Unknown
Journal Title
Glass International May 2014 3
Sector
News Items
Class
N 3268

Request article (free for British Glass members)

Tiama Partnership
Glass International May 2014 3
N 3268
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.