Tiama Group Introduces Its Multi-Inspection Carousel Platform - The Mx

This year's edition of glasstec was a great opportunity for MSC and SGCC to introduce the MX, the latest carousel platform launched by Tiama, the main provider of online process and quality improvement solutions for glassmakers. The MX was developed to offer a unique carousel solution. It is a merger of all MSC and SGCC know-how regarding multi-inspection solutions built over years with the CO, M1 and CHECK+ market references. MX performs a complete range of measurement and controls in accordance to glass plant needs: detection and measurement of dimensional defects (finish and neck), crack detection by cameras, non-contact thickness measurement, airtightness measurement, non-contact ovalization, mould number reading and detection of visual defects in specific areas. For more information, please visit: www.msc-sgcc.com

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 6/12 20-23
Sector
Container glass
Class
C 4828

Request article (free for British Glass members)

Tiama Group Introduces Its Multi-Inspection Carousel Platform - The Mx
Gmpa 6/12 20-23
C 4828
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.